The fire-resistant function of frameless fire-proof glass for construction is obtained by embedding frameless fire-proof glass directly in the wall hole or combined with the structure, and then embedded in the wall hole to make components according to gbl2513. It includes the determination of fire-resistant integrity, fire-resistant heat insulation and thermal radiation intensity. Meanwhile, the measurement of thermal insulation is based on the back fire surface temperature.
Fire resistance and thermal insulation refers to the temperature rise of single point at the temperature measuring point on the back fire surface of the test piece of 180 ℃ and uniform temperature rise of 140 ℃.
Thermal radiation intensity refers to the critical radiant heat illuminance of 0.42w/cm2 at 3M away from the back fire surface of the test piece, and the critical radiant heat illuminance of 3.35 w / cm2 at an interval equal to 1.2 times its smaller scale (length or width) from the back fire surface of the test piece. Fire resistance function test: the whole frameless fireproof glass shall be embedded in the fixed structure, and the fire resistance function test shall be carried out according to gb12513. The fire resistance scale of frameless fireproof glass shall not be less than 1100mm high and 600mm wide, and the sample shall be straight. The fixed structure and device method used in the experiment shall be the same as the structure used in the actual project, and the structure and device method of the fixed structure shall be recorded in the way of drawings.
Bending test: place the glass pen vertically, place the ruler horizontally close to the surface of the sample for measurement, and indicate it in the percentage of the ratio of the height of the arc to the length of the chord when it is arched; The waveform is indicated by the percentage of the ratio of the height from trough to peak to the interval from peak to peak (or trough to trough). The products shall be packed in wooden cases or other packing boxes. The glass pen shall be placed vertically in the box. Each glass shall be wrapped with plastic cloth or paper. The light and soft materials that are not easy to cause glass scratches and other appearance defects shall be filled between the glass and the packing box.
Article source: fireproof glass http://twqwq.cn/
05-04
What are the problems of composite fireproof glass in fire fighting
Some supervisors mistakenly think that the door made of fireproof glass is the fireproof door, the partition made of fireproof glass is the fireproof glass partition, and the window made of fireproof
04-12
Fireproof glass door: how to ensure that the fireproof door can play a role in critical times
How to ensure that the fire door can give full play to its ideal effect in critical time?1. Select appropriate typesAccording to the relevant specific introduction of fire doors, we can know that at t
02-17
Where is the fireproof glass generally installed
(1) the fireproof glass is generally installed on something. It may not be checked from time to time before installation. If the warpage, unsightness and glass hazards of the window edge and window ar
10-30
How to distinguish the quality of single fireproof glass?
1. Equipment conditions:No matter how to make a single piece of fireproof glass, it can't be done without some equipment, so if the manufacturer doesn't have the equipment, it can't mak